A method for measurement of triboelectric charging has been defined. The principle of the method is measurement by an electrostatic voltmeter of the voltage developed on a test piece when after a roll has rolled over it. The used roll materials are quartz and teflon respectively. Other materials can be used but are not verified in this work. The method is evaluated to give a repeatability when measuring electrostatic conductive foils to better than ± 10 % (1σ). This figure includes spread in the test item itself. Before being proposed as a standard the method has to be further evaluated. The development has been performed step-by-step and possibly the method could be simplified by repeating some of these when reference is given by this work. Comparative measurements ("Round Robin tests") should be performed by other laboratories to evaluate the reproducability of the method. To facilitate the method and possibly adapt it better to a "real-life" situation the theoretical physical phenomena behind the electrostatic charging mechanism, the relaxation behaviour of the roll and the dependence of the roll surface smoothness should be better clarified.
SP REPORT 1994:34