PVC flooring systems exposed to humid and alkaline conditions have been studied during extended periods of time both in the field and in the laboratory. PVC sheets were glued to both raw and concrete surfaces and were protected by different kinds of moisture barriers. Underneath, the concrete slabs were either exposed to sand saturated with water or 100 % RH. The relative humidity was determined with a measuring device intended for measuring between the moisture barrier and the flooring. Moisture barriers of conventional thickness (<= 200 m) did not restrain moisture penetration. However, alkali resistant materials could serve as alkali barriers and protect the adhesive layer and PVC flooring from degradation up to at least 1.5 years. Some moisture barriers were not alkali resistant and could not protect the upper layers from alkaline hydrolysis. An evident smell of octanol was observed and the flooring showed staining. Without moisture barrier the glue was rapidly destroyed. The floor showed staining and smelled of octanol.
SP Rapport 1989:07