Properties of wheat gluten/poly(lactic acid) laminates
RISE., Innventia.
RISE., Innventia.
2010 (Engelska)Ingår i: Journal of Agricultural and Food Chemistry, ISSN 0021-8561, E-ISSN 1520-5118, Vol. 58, nr 12, s. 7344-7350Artikel i tidskrift (Refereegranskat) Published
Abstract [en]

Laminates of compression-molded glycerol-plasticized wheat gluten (WG) films surrounded and supported by poly(lactic acid) (PLA) films have been produced and characterized. The objective was to obtain a fully renewable high gas barrier film with sufficient mechanical integrity to function in, for example, extrusion-coating paper/board applications. It was shown that the lamination made it possible to make films with a broad range of glycerol contents (0-30 wt %) with greater strength than single unsupported WG films. The low plasticizer contents yielded laminates with very good oxygen barrier properties. In addition, whereas the unsupported WG films had an immeasurably high water vapor transmission rate (WVTR), the laminate showed values that were finite and surprisingly, in several cases, also lower than that of PLA. Besides being a mechanical support (as evidenced by bending and tensile data) and a shield between the WG and surrounding moisture, the PLA layer also prevented the loss of the glycerol plasticizer from the WG layer. This was observed after the laminate had been aged on an "absorbing" blotting paper for up to 17 weeks. The interlayer adhesion (peel strength) decreased with decreasing glycerol content and increasing WG film molding temperature (130 °C instead of 110 °C). The latter effect was probably due to a higher protein aggregation, as revealed by infrared spectroscopy. The lamination temperature (110-140 °C) did not, however, have a major effect on the final peel strength.

Ort, förlag, år, upplaga, sidor
2010. Vol. 58, nr 12, s. 7344-7350
Nyckelord [en]
Biopolymer, Glycerol content, Laminate, Oxygen permeability, Poly(lactic acid), Water vapor transmission rate, Wheat gluten
Nationell ämneskategori
Kompositmaterial och -teknik
Identifikatorer
URN: urn:nbn:se:ri:diva-29560DOI: 10.1021/jf1003144Scopus ID: 2-s2.0-77953624673OAI: oai:DiVA.org:ri-29560DiVA, id: diva2:1095699
Anmärkning

cited By 14

Tillgänglig från: 2017-05-15 Skapad: 2017-05-15 Senast uppdaterad: 2025-09-23Bibliografiskt granskad

Open Access i DiVA

Fulltext saknas i DiVA

Övriga länkar

Förlagets fulltextScopus
Av organisationen
Innventia
I samma tidskrift
Journal of Agricultural and Food Chemistry
Kompositmaterial och -teknik

Sök vidare utanför DiVA

GoogleGoogle Scholar

doi
urn-nbn

Altmetricpoäng

doi
urn-nbn
Totalt: 115 träffar
RefereraExporteraLänk till posten
Permanent länk

Direktlänk
Referera
Referensformat
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Annat format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annat språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf