Bone response to physical-vapour-deposited titanium dioxide coatings on titanium implants
Sahlgrenska Academy, Sweden.
Sandvik, Sweden.
Sandvik, Sweden.
Sahlgrenska Academy, Sweden.
Show others and affiliations
2013 (English)In: Clinical Oral Implants Research, ISSN 0905-7161, E-ISSN 1600-0501, Vol. 24, no 9, p. 1009-1017Article in journal (Refereed) Published
Abstract [en]

Objectives: The aim of this study was to investigate the correlation between coating thickness and the crystal structure of physical-vapour-deposited (PVD) titanium dioxide coatings, and to evaluate their in vivo biocompatibility. Materials and methods: The PVD TiO 2 coatings of different thickness were deposited on machined titanium grade 2 screw-shaped implants. Non-coated titanium implants were used as controls. Coating properties such as thickness, crystal structure, coating morphology and roughness were characterized. Forty-eight implants were placed randomly into both tibias of 16 rats. The animals were euthanized 7 and 28 days postsurgery and block biopsies were prepared for histology, histomorphometry and SEM analysis. Results: The thicknesses of the PVDTiO 2 coatings were 120 and 1430 nm respectively. Histologically, new bone formed on all implant surfaces. The mean percentage of newly formed bone in contact with the implant (BIC) was significantly higher at early healing time (7 days) for the 120 nm thick PVD coating (39 ± 14%) than for both the 1430 nm thick PVD coating (22 ± 10%) (P = 0.043) and the machined surface (22 ± 9%) (P = 0.028). This difference was no longer evident after 28 days (P = 0.867). Conclusion: Bone formation and bone-to-implant contact are achieved to the same degree for TiO 2 surface modifications prepared by a PVD process as clinically used, machined titanium. Furthermore, a relatively thinner PVD coating promotes a higher degree of bone apposition shortly after implantation, thereby providing rationales for exploring the potential clinical use of these modifications.

Place, publisher, year, edition, pages
2013. Vol. 24, no 9, p. 1009-1017
National Category
Natural Sciences
Identifiers
URN: urn:nbn:se:ri:diva-6594DOI: 10.1111/j.1600-0501.2012.02509.xScopus ID: 2-s2.0-84880845286Local ID: 23897OAI: oai:DiVA.org:ri-6594DiVA, id: diva2:964433
Available from: 2016-09-08 Created: 2016-09-08 Last updated: 2020-12-01Bibliographically approved

Open Access in DiVA

No full text in DiVA

Other links

Publisher's full textScopus

Authority records

Lausmaa, Jukka

Search in DiVA

By author/editor
Lausmaa, Jukka
By organisation
SP – Sveriges Tekniska Forskningsinstitut / Funktionella material (KMf)
In the same journal
Clinical Oral Implants Research
Natural Sciences

Search outside of DiVA

GoogleGoogle Scholar

doi
urn-nbn

Altmetric score

doi
urn-nbn
Total: 64 hits
CiteExportLink to record
Permanent link

Direct link
Cite
Citation style
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Other style
More styles
Language
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Other locale
More languages
Output format
  • html
  • text
  • asciidoc
  • rtf