The impact of coating hardness on the anti-barnacle efficacy of an embedded antifouling biocide
RISE., SP – Sveriges Tekniska Forskningsinstitut, SP Kemi Material och Ytor, Medicinteknik. University of Gothenburg, Sweden.ORCID-id: 0000-0002-8945-9904
University of Gothenburg, Sweden.
RISE., SP – Sveriges Tekniska Forskningsinstitut, SP Kemi Material och Ytor, Material och ytteknik. University of Gothenburg, Sweden.ORCID-id: 0000-0002-9377-8924
2013 (Engelska)Ingår i: Biofouling (Print), ISSN 0892-7014, E-ISSN 1029-2454, Vol. 29, nr 7, s. 763-773Artikel i tidskrift (Refereegranskat) Published
Abstract [en]

The efficacy of antifouling coatings designed to minimise the release of biocide, either by embedded (non-covalent) or tethered (covalently bonded) biocides, relies on sufficient bioavailability of the active compound upon contact between the organism and the coating. This investigation is focused on whether coating hardness affects the efficacy of embedded coating systems. Two experimental, non-eroding and waterborne latex paint formulations composed mainly of polystyrene (PS) or polyvinyl versatate (PV) were chosen for their difference in mechanical properties measured in terms of Buchholz indentation resistance. Ivermectin was added to both formulations to a final concentration of 0.1% (w/v) and the steady state release rate was measured according to ISO 15181 at between 34 and 70 ng cm-2 day-1 for both formulations. Field trials conducted over 3 months showed significant differences in anti-barnacle efficacy between the formulations despite their similar release profiles. The softer PV coating showed complete anti-barnacle efficacy, ie no barnacles were detected, while the harder PS coating showed no efficacy against barnacle colonisation during the same time period. The results indicate a new antifouling strategy whereby a route of intoxication is triggered by the organism itself upon interaction with the coating and its embedded biocide. This finding opens new possibilities in controlling macrofouling by low emission antifouling coatings.

Ort, förlag, år, upplaga, sidor
2013. Vol. 29, nr 7, s. 763-773
Nyckelord [en]
barnacle, coating hardness, coating penetration, contact active antifouling, embedded biocidelow emission antifouling
Nationell ämneskategori
Naturvetenskap
Identifikatorer
URN: urn:nbn:se:ri:diva-6544DOI: 10.1080/08927014.2013.804511Scopus ID: 2-s2.0-84880510613Lokalt ID: 23825OAI: oai:DiVA.org:ri-6544DiVA, id: diva2:964382
Tillgänglig från: 2016-09-08 Skapad: 2016-09-08 Senast uppdaterad: 2023-05-25Bibliografiskt granskad

Open Access i DiVA

Fulltext saknas i DiVA

Övriga länkar

Förlagets fulltextScopus

Person

Pinori, EmilianoBerglin, Mattias

Sök vidare i DiVA

Av författaren/redaktören
Pinori, EmilianoBerglin, Mattias
Av organisationen
MedicinteknikMaterial och ytteknik
I samma tidskrift
Biofouling (Print)
Naturvetenskap

Sök vidare utanför DiVA

GoogleGoogle Scholar

doi
urn-nbn

Altmetricpoäng

doi
urn-nbn
Totalt: 91 träffar
RefereraExporteraLänk till posten
Permanent länk

Direktlänk
Referera
Referensformat
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Annat format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annat språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf