The Effect of Accelerated Ageing on Reaction-to-Fire Properties–Composite Materials
RISE Research Institutes of Sweden, Säkerhet och transport, Brandteknik. DTU Technical University of Denmark, Denmark.ORCID-id: 0000-0002-7001-9757
RISE Research Institutes of Sweden, Säkerhet och transport, Brandteknik.ORCID-id: 0000-0002-6430-6602
DTU Technical University of Denmark, Denmark.
RISE Research Institutes of Sweden, Säkerhet och transport, Säkerhetsforskning. DTU Technical University of Denmark, Denmark.ORCID-id: 0000-0002-6120-2461
2022 (engelsk)Inngår i: Fire technology, ISSN 0015-2684, E-ISSN 1572-8099, Vol. 58, nr 3, s. 1305-1332Artikkel i tidsskrift (Fagfellevurdert) Published
Abstract [en]

As material age, the durability, strength, and other mechanical properties are impacted. The lifespan of a material generally decreases when exposed to weathering conditions such as wind, temperature, humidity, and light. It is important to have knowledge of how materials age and how the material properties are affected. Regarding materials´ fire behaviour and the effect of ageing on these properties, the knowledge is limited. The research questions of the current work are: Are the fire properties of composite materials affected by ageing? And if so, how is it affected? The study is on material at Technology Readiness Level 9 (TRL). In this study, three composite fibre laminates developed for marine applications were exposed to accelerated ageing. Two different ageing conditions were selected, thermal ageing with an increased temperature of 90°C and moisture ageing in a moderately increased temperature of 40°C and a relative humidity of 90%. Samples were collected after one, two and four weeks of ageing. The reaction-to-fire properties after ageing was evaluated using the ISO 5660–1 cone calorimeter and the EN ISO 5659–2 smoke chamber with FTIR gas analysis. The test results showed that the fire behaviour was affected. Two of the composite laminates, both phenolic/basalt composites, showed a deteriorated fire behaviour from the thermal ageing and the third composite laminate, a PFA/glass fibre composite, showed an improved fire behaviour both for thermal and moisture ageing. The smoke toxicity was affected by the accelerated ageing, especially for the PFA/glass fibre composite that showed a higher production of CO and HCN, both for the thermal aged and the moisture aged samples. © 2021, The Author(s).

sted, utgiver, år, opplag, sider
Springer , 2022. Vol. 58, nr 3, s. 1305-1332
Emneord [en]
Accelerated ageing, Composite laminates, Cone calorimeter, Moisture exposure, Reaction-to-fire, Smoke density, Thermal exposure, Toxicity, Durability, Fires, Laminated composites, Marine applications, Smoke, %moisture, Composite laminate, Fire behaviour, Fire properties, Reaction to fire, Moisture
HSV kategori
Identifikatorer
URN: urn:nbn:se:ri:diva-57366DOI: 10.1007/s10694-021-01197-9Scopus ID: 2-s2.0-85119970365OAI: oai:DiVA.org:ri-57366DiVA, id: diva2:1621329
Merknad

Funding details: Horizon 2020 Framework Programme, H2020, 723246; Funding text 1: The research presented is a part of the RAMSSES project which has received funding under the European Union’s Horizon 2020 research and innovation programme under the grant agreement No 723246.

Tilgjengelig fra: 2021-12-17 Laget: 2021-12-17 Sist oppdatert: 2023-06-05bibliografisk kontrollert

Open Access i DiVA

Fulltekst mangler i DiVA

Andre lenker

Forlagets fulltekstScopus

Person

Sandinge, AnnaBlomqvist, PerDederichs, Anne

Søk i DiVA

Av forfatter/redaktør
Sandinge, AnnaBlomqvist, PerDederichs, Anne
Av organisasjonen
I samme tidsskrift
Fire technology

Søk utenfor DiVA

GoogleGoogle Scholar

doi
urn-nbn

Altmetric

doi
urn-nbn
Totalt: 91 treff
RefereraExporteraLink to record
Permanent link

Direct link
Referera
Referensformat
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Annet format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annet språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf
v. 2.43.0