Stability and aging resistance of a zirconia oral implant using a carbon fiber-reinforced screw for implant-abutment connection
University of Freiburg, Germany; Humboldt-Universität zu Berlin, Germany.
University of Freiburg, Germany.
RISE - Research Institutes of Sweden, Materials and Production, IVF.ORCID iD: 0000-0003-4860-8763
University of Freiburg, Germany.
Show others and affiliations
2018 (English)In: Dental Materials, ISSN 0109-5641, E-ISSN 1879-0097, Vol. 34, no 10, p. 1585-1595Article in journal (Refereed) Published
Abstract [en]

OBJECTIVE: To investigate the long-term stability of a metal-free zirconia two-piece implant assembled with a carbon fiber-reinforced (CRF) screw by means of transformation propagation, potential changes in surface roughness, the gap size of the implant-abutment connection, and fracture load values.

METHODS: In a combined procedure, two-piece implants made from alumina-toughened zirconia were dynamically loaded (107 cycles) and hydrothermally aged (85°, 60days). Implants made from titanium (Ti) and a titanium-zirconium (TiZr) alloy with a titanium abutment screw served as control. Transformation propagation (ATZ) and gap size of the IAC were monitored at cross-sections by scanning electron microscopy (SEM). Furthermore, changes in surface roughness of ATZ implants were measured. Finally, implants were statically loaded to fracture. Linear regression models and pairwise comparisons were used for statistical analyses.

RESULTS: Independent of the implant bulk material, dynamic loading/hydrothermal aging did not decrease fracture resistance (p=0.704). All test and control implants fractured at mean loads >1100N. Gap size of the IAC remained stable (<5μm) or decreased. None of the CFR screws fractured during static or dynamic loading. Monoclinic layer thickness of ATZ implants increased by 2-3μm at surfaces exposed to water, including internal surfaces of the IAC. No changes in surface roughness were observed.

SIGNIFICANCE: Combined hydrothermal aging and dynamic loading did not affect the above-mentioned parameters of the evaluated two-piece ATZ implant. Mean fracture loads >1100N suggest a reliable clinical application.

Place, publisher, year, edition, pages
2018. Vol. 34, no 10, p. 1585-1595
Keywords [en]
Ceramics, Crystallography, Dental implant, Scanning electron microscopy, Zirconia
National Category
Natural Sciences
Identifiers
URN: urn:nbn:se:ri:diva-35141DOI: 10.1016/j.dental.2018.08.290PubMedID: 30180975Scopus ID: 2-s2.0-85052797091OAI: oai:DiVA.org:ri-35141DiVA, id: diva2:1247172
Available from: 2018-09-11 Created: 2018-09-11 Last updated: 2019-06-17Bibliographically approved

Open Access in DiVA

No full text in DiVA

Other links

Publisher's full textPubMedScopus

Authority records

Adolfsson, Erik

Search in DiVA

By author/editor
Adolfsson, Erik
By organisation
IVF
In the same journal
Dental Materials
Natural Sciences

Search outside of DiVA

GoogleGoogle Scholar

doi
pubmed
urn-nbn

Altmetric score

doi
pubmed
urn-nbn
Total: 42 hits
CiteExportLink to record
Permanent link

Direct link
Cite
Citation style
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Other style
More styles
Language
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Other locale
More languages
Output format
  • html
  • text
  • asciidoc
  • rtf