Surface modification of solid wood by charringShow others and affiliations
2017 (English)In: Journal of Materials Science, ISSN 0022-2461, E-ISSN 1573-4803, Vol. 52, no 10, p. 6111-6119Article in journal (Refereed) Published
Abstract [en]
Most wooden structures for outdoor applications require repetitive maintenance operations to protect the surfaces from adverse effects of weathering. One-sided surface modification of boards with a relatively fast charring process has the potential to increase the durability and service life of wooden claddings. To assess some weathering-related effects on surface charred wood, spruce and pine sapwood were subjected to a series of long charring processes (30â120 min) at a moderate temperature of 250 °C and to a short one (30 s) at a high temperature of 400 °C. The wettability and contact angles of treated samples were investigated, and the heat transfer was measured along with the micromorphological changes taking place in the material. The result revealed an increased moisture resistance of charred spruce sapwood and an increased water uptake of pine sapwood. The contact angles of both wood species improved compared to references. Heat conduction measurement revealed that only a thin section of the wood was thermally modified. Some micromorphological changes were recorded, especially on the inside walls of the lumina. The results show that spruce sapwood has an improved resistance towards moisture-induced weathering, but more studies are needed to unlock the potential of surface charred wood.
Place, publisher, year, edition, pages
2017. Vol. 52, no 10, p. 6111-6119
Keywords [en]
solid wood, contact angle, heat conduction, heat transfer, moisture, surface treatment, weathering, wood product, wooden building
National Category
Wood Science
Identifiers
URN: urn:nbn:se:ri:diva-30340DOI: 10.1007/s10853-017-0850-yScopus ID: 2-s2.0-85011878891OAI: oai:DiVA.org:ri-30340DiVA, id: diva2:1134283
2017-08-182017-08-182019-12-12Bibliographically approved