  • html
  • text
  • asciidoc
  • rtf
Micro-galvanic corrosion effects on patterned copper-zinc samples during exposure in humidified air containing formic acid
KTH Royal Institute of Technology, Sweden.
KTH Royal Institute of Technology, Sweden.
RISE., SP – Sveriges Tekniska Forskningsinstitut.
Xiamen University, China.
Visa övriga samt affilieringar
2013 (Engelska)Ingår i: Journal of the Electrochemical Society, ISSN 0013-4651, E-ISSN 1945-7111, Vol. 160, nr 9, s. C423-C431Artikel i tidskrift (Refereegranskat) Published
Abstract [en]

Corrosion in indoor atmospheric environments is often triggered by carboxylic acids, especially at higher relative humidity. Microgalvanic effects can lead to severe corrosion, particularly important in miniature devices with small-sized metallic components. To elucidate the mechanism of micro-galvanic corrosion effects, well-defined zinc-copper patterned samples were investigated during exposure to 100 ppb formic acid (HCOOH) and 80% relative humidity at 20°C. The corrosion effects were monitored quantitatively with in situ infrared absorption spectroscopy, and the corrosion products characterized with scanning electron microscopy, confocal Raman microscopy, and atomic force microscopy. The nature of corrosion on zinc on the patterned samples was compared with that on pure zinc and turned out to result, not only in several times higher corrosion kinetics, but also in different corrosion products with respect to distribution, morphology, and composition. Local electrochemical and chemical gradients across the copper-zinc borders resulted in characteristic hemispherically shaped corrosion products at the zinc-copper junction, and in the formation of zinc formate dihydrate (Zn(HCOO)2 · 2H 2O) and crystalline zinc oxide (ZnO), phases not identified on pure zinc. In all, the micro-galvanic effects on the patterned samples resulted in accelerated corrosion kinetics and in structurally more developed corrosion products.

Ort, förlag, år, upplaga, sidor
2013. Vol. 160, nr 9, s. C423-C431
Nationell ämneskategori
Naturvetenskap
Identifikatorer
URN: urn:nbn:se:ri:diva-6582DOI: 10.1149/2.113308jesScopus ID: 2-s2.0-84881512858Lokalt ID: 23879OAI: oai:DiVA.org:ri-6582DiVA, id: diva2:964421
Tillgänglig från: 2016-09-08 Skapad: 2016-09-08 Senast uppdaterad: 2020-12-01Bibliografiskt granskad

Open Access i DiVA

Fulltext saknas i DiVA

Övriga länkar

Förlagets fulltextScopus
Av organisationen
SP – Sveriges Tekniska Forskningsinstitut
I samma tidskrift
Journal of the Electrochemical Society
Naturvetenskap

Sök vidare utanför DiVA

GoogleGoogle Scholar

doi
urn-nbn

Altmetricpoäng

doi
urn-nbn
Totalt: 54 träffar
RefereraExporteraLänk till posten
Permanent länk

Direktlänk
Referera
Referensformat
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Annat format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annat språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf