Corrosion performance of Zn-Al-Mg coatings in open and confined zones in conditions simulating automotive applications
RISE - Research Institutes of Sweden (2017-2019), Material och produktion, KIMAB. (Institut de la Corrosion)
RISE - Research Institutes of Sweden (2017-2019), Material och produktion, KIMAB. (Institut de la Corrosion)
Corus, The Netherlands.
IZA, USA.
Visa övriga samt affilieringar
2010 (Engelska)Ingår i: Materials and corrosion - Werkstoffe und Korrosion, ISSN 0947-5117, E-ISSN 1521-4176, Vol. 61, nr 5, s. 412-420Artikel i tidskrift (Refereegranskat) Published
Abstract [en]

Panels coated by hot dipping with zinc (HDG), Zn-5Al (Galfan) and Zn-1.5Al- 1.5Mg coatings at different thicknesses were phosphated and painted on an industrial line. Crevice panels with non-painted bare parts modelling conditions in hem flanges, reference panels with open surfaces and formed non-painted panels were exposed to a cyclic accelerated automotive test. Zn-Al-Mg coatings with the thickness of 10 μ rovided similar or even better protection than HDG and Galfan at 20 mmin both confined and open configurations. In comparison to 10-μm HDG, the Zn-Al-Mg coating delayed red rust appearance in crevices by a factor of 2 and the maximal depth of corrosion in the steel substrate was by 42% lower. Confined areas were more corroded than open surfaces. For HDG, the time to red rust appearance dropped by 50-75%, corrosion attack in steel was from 3.5 to 7 times deeper and mass gain was about 2.3 times higher in crevices than on open surfaces. Corrosion of Zn-Al-Mg may be more affected by local environmental conditions created by the crevice configuration than for HDG. Red rust appearance on formed panels of 20-mm Galfan, 7-, 10- and 14-mm Zn- Al-Mg was delayed to 10-μm HDG by a factor of 2.8, 3.5, 3.8 and >4.5, respectively. No adverse effect of forming was noticed. The results indicate that 2- to 3-fold reduction of the coating thickness for Zn-Al-Mg alloy coatings in comparison to traditional HDG may be possible without compromising the corrosion performance.

Ort, förlag, år, upplaga, sidor
2010. Vol. 61, nr 5, s. 412-420
Nyckelord [en]
Adverse effect, Al-Mg alloy, Automotive applications, Coating thickness, Confined areas, Corrosion attack, Corrosion performance, Environmental conditions, Hot dipping, Mass gain, Rust appearance, Steel substrate, Coatings, Corrosion, Thickness measurement, Zinc, Zinc alloys, Zinc coatings, Aluminum
Nationell ämneskategori
Teknik och teknologier
Identifikatorer
URN: urn:nbn:se:ri:diva-40423DOI: 10.1002/maco.200905425Scopus ID: 2-s2.0-77952993874OAI: oai:DiVA.org:ri-40423DiVA, id: diva2:1361399
Tillgänglig från: 2019-10-16 Skapad: 2019-10-16 Senast uppdaterad: 2023-05-16Bibliografiskt granskad

Open Access i DiVA

Fulltext saknas i DiVA

Övriga länkar

Förlagets fulltextScopus

Person

Thierry, Dominique

Sök vidare i DiVA

Av författaren/redaktören
Thierry, Dominique
Av organisationen
KIMAB
I samma tidskrift
Materials and corrosion - Werkstoffe und Korrosion
Teknik och teknologier

Sök vidare utanför DiVA

GoogleGoogle Scholar

doi
urn-nbn

Altmetricpoäng

doi
urn-nbn
Totalt: 27 träffar
RefereraExporteraLänk till posten
Permanent länk

Direktlänk
Referera
Referensformat
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Annat format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annat språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf