Ytterbium-doped fibers fabricated with atomic layer deposition method Visa övriga samt affilieringar
2012 (Engelska) Ingår i: Optics Express, E-ISSN 1094-4087, Vol. 20, nr 22, s. 25085-95Artikel i tidskrift (Refereegranskat) Published
Abstract [en]
We report on a new fabrication method of producing ytterbium doped fibers by atomic layer deposition (ALD) in combination with the conventional modified chemical vapor deposition (MCVD) technique. An MCVD soot-preform with a porous layer of SiO2 is coated with layers of Yb2O3 and Al2O3 prior to sintering, using the gas-phase ALD method. An SEM/EDS material analysis study shows that the dopants successfully penetrate the full thickness of 320 μm of the soot layer. An Yb-doped fiber fabricated by this technique shows a background attenuation of 20 dB/km, a uniform longitudinal Yb-doping profile, and good laser characteristics with a slope efficiency of 80%. Furthermore, we present a comparison in terms of photodarkening between the MCVD-ALD fiber and a solution doped fiber, fabricated with the same MCVD recipe. The new MCVD-ALD fiber appears to be more photodarkening resistant.
Ort, förlag, år, upplaga, sidor 2012. Vol. 20, nr 22, s. 25085-95
Nyckelord [en]
Atomic layer, Doped fiber, Fabrication method, Gasphase, Laser characteristics, Material analysis, Modified chemical vapor depositions, Porous layers, SEM/EDS, Slope efficiencies, Yb-doped fibers, Yb-doping, Ytterbium doped fibers
Nationell ämneskategori
Data- och informationsvetenskap
Identifikatorer URN: urn:nbn:se:ri:diva-32009 DOI: 10.1364/OE.20.025085 Scopus ID: 2-s2.0-84868261174 OAI: oai:DiVA.org:ri-32009 DiVA, id: diva2:1151867
2017-10-242017-10-242022-09-15 Bibliografiskt granskad