Corrosion of superheater materials in a waste-to-energy plant
RISE, Swerea, Swerea KIMAB AB.
2013 (engelsk)Konferansepaper, Publicerat paper (Fagfellevurdert)
Abstract [en]

A major drawback when generating electricity from waste-fired boilers is the rapid corrosion of critical components such as superheater tubes. In this work a number of commonly-used superheater materials have been exposed on internally cooled probes in a waste-fired grate boiler. The investigated materials are the ferritic steel 13CrMo44, the ferritic-martensitic steel HCM12A, the austenitic steels Super 304, 317L and Sanicro 28, and the nickel-base alloys Hastelloy C-2000 and Inconel 625. Short-term exposures (3 h) for analysis of deposit composition and initial corrosion, as well as long-term exposures (1550 h) to investigate corrosion rates and corrosion characteristics have been made. Analysis revealed a deposit dominated by CaSO 4, KCl and NaCl, but also appreciable amounts of low melting salt mixtures such as ZnCl 2-KCl, PbCl 2-KCl, FeCl 2-KCl and NaCl-NiCl 2. Metal loss measurements showed unacceptably high corrosion rates for 13CrMo44, HCM12A and Super 304. The corrosion attack for these alloys was manifested by the formation of mixed metal chloride/metal oxide scales. A different type of behaviour was seen for the higher alloyed austenitic steels and nickel-base alloys, which were able to form a chromium-enriched oxide next to the metal. However, these alloys suffered from some localised pitting attack. The behaviour is explained by oxide dissolution in the molten salts that are present in the deposit. © 2011 Elsevier B.V.

sted, utgiver, år, opplag, sider
2013. Vol. 105, s. 106-112
Serie
Fuel Processing Technology, ISSN 0378-3820
Emneord [en]
Deposits, High temperature corrosion, Waste incineration
HSV kategori
Identifikatorer
URN: urn:nbn:se:ri:diva-12931DOI: 10.1016/j.fuproc.2011.06.017OAI: oai:DiVA.org:ri-12931DiVA, id: diva2:973124
Tilgjengelig fra: 2016-09-22 Laget: 2016-09-22bibliografisk kontrollert

Open Access i DiVA

Fulltekst mangler i DiVA

Andre lenker

Forlagets fullteksthttp://www.scopus.com/inward/record.url?eid=2-s2.0-84869089947&partnerID=40&md5=c3b1ff8da3572f394c4dd4ef3179d27b
Av organisasjonen

Søk utenfor DiVA

GoogleGoogle Scholar

doi
urn-nbn

Altmetric

doi
urn-nbn
Totalt: 42 treff
RefereraExporteraLink to record
Permanent link

Direct link
Referera
Referensformat
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Annet format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annet språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf
v. 2.41.0