Corrosion behavior of a Mo(Si, Al)2 composite at 1700°C in 95% N2 + 5% H2
RISE - Research Institutes of Sweden, Material och produktion, IVF.
RISE - Research Institutes of Sweden, Bioekonomi, ETC Energy Technology Center.ORCID-id: 0000-0002-6473-7090
RISE - Research Institutes of Sweden, Material och produktion, IVF.
RISE - Research Institutes of Sweden, Material och produktion, IVF.
Vise andre og tillknytning
2019 (engelsk)Inngår i: Journal of the European Ceramic Society, ISSN 0955-2219, E-ISSN 1873-619X, Vol. 39, nr 16, s. 5197-5203Artikkel i tidsskrift (Fagfellevurdert) Published
Abstract [en]

A Mo(Si, Al)2 based composite was pre-oxidized to establish an alumina scale on the material surface. Thereafter, the corrosion behavior of the composite was examined at 1700 °C for up to 24 h in 95% N2 + 5% H2. The weight change was followed by recording the material weight before and after exposure. The crystalline corrosion products were analyzed with X-ray diffraction (XRD) and the microstructure of the cross sectioned material was characterized using scanning electron microscopy (SEM) with energy dispersive X-ray spectroscopy (EDS). It was shown that AlN and Al5O6N layers developed on top of the pre-oxidized alumina layer and alumina threads develop out from the specimen surface. The accompanied aluminum consumption converts the substrate Mo(Si,Al)2 into Mo5Si3 immediately below the alumina scale to the extent that the Mo5Si3 becomes porous underneath the alumina scale. Corrosion mechanisms are discussed with the support of thermodynamic calculations.

sted, utgiver, år, opplag, sider
Elsevier Ltd , 2019. Vol. 39, nr 16, s. 5197-5203
Emneord [en]
Alumina, High temperature corrosion, Mo(Si, Al)2, Molybdenum disiliside, Nitrogen, Aluminum nitride, Aluminum oxide, Corrosive effects, Energy dispersive spectroscopy, III-V semiconductors, Molybdenum compounds, Scanning electron microscopy, Alumina layers, Corrosion behavior, Corrosion mechanisms, Corrosion products, Energy dispersive X ray spectroscopy, Material surface, Specimen surfaces, Thermodynamic calculations, Aluminum corrosion
HSV kategori
Identifikatorer
URN: urn:nbn:se:ri:diva-39849DOI: 10.1016/j.jeurceramsoc.2019.08.017Scopus ID: 2-s2.0-85070899991OAI: oai:DiVA.org:ri-39849DiVA, id: diva2:1347264
Tilgjengelig fra: 2019-08-30 Laget: 2019-08-30 Sist oppdatert: 2020-01-29bibliografisk kontrollert

Open Access i DiVA

Fulltekst mangler i DiVA

Andre lenker

Forlagets fulltekstScopus

Person

Ögren, Yngve

Søk i DiVA

Av forfatter/redaktør
Ögren, Yngve
Av organisasjonen
I samme tidsskrift
Journal of the European Ceramic Society

Søk utenfor DiVA

GoogleGoogle Scholar

doi
urn-nbn

Altmetric

doi
urn-nbn
Totalt: 107 treff
RefereraExporteraLink to record
Permanent link

Direct link
Referera
Referensformat
  • apa
  • ieee
  • modern-language-association-8th-edition
  • vancouver
  • Annet format
Fler format
Språk
  • de-DE
  • en-GB
  • en-US
  • fi-FI
  • nn-NO
  • nn-NB
  • sv-SE
  • Annet språk
Fler språk
Utmatningsformat
  • html
  • text
  • asciidoc
  • rtf
v. 2.46.0